Catalyst of diphenylamine
LSCD-A
Item |
unit |
target |
|
Technical parameter |
Shape |
|
white column |
Diameter |
mm |
1.8-2.5 |
|
Length |
mm |
5-13 |
|
Bulk density |
g/ml |
60-70/100 |
|
surface area |
㎡/g |
440-490 |
|
Pore bulk |
ml/g |
0.35-0.5 |
|
Compressive strength |
N/mm |
﹥7 |
|
Performance |
Reaction tempreture |
℃ |
320-325 |
Reaction pression |
mpa |
1.8-2.2 |
|
Airspeed |
h-1 |
0.2-0.22 |
|
Content of Diphenylamine |
% |
≥21 |
|
Selectivity |
% |
≥98 |
|
One-pass life |
h |
>1500 |
Comment: Airspeed is measured every 2 hour after the reaction react 100h.
LSCD-B Catalyst of diphenylamine is synthesized using nanocrystalline siallitic oxide and nano-fibers as raw staff. The technical parameter of catalyst of LSCD-B is more excellent than LSCD-A, such as surface area, pore distribution and pore size so on. The performance parameter of LSCD-B is shown as follow.
Item |
unit |
target |
|
Performance |
Reaction tempreture |
℃ |
316-322 |
Reaction pression |
mpa |
2.0 |
|
Airspeed |
h-1 |
0.4-0.5 |
|
Content of Diphenylamine |
% |
≥31 |
|
Selectivity |
% |
≥97 |
|
One-pass life |
h |
>2000 |
Comment: Airspeed is measured every 4 hour after the reaction react 100h